25% SIC BASED BRICKS |
Properties | Value | SB25S001A (25%) | SB25S002A (23-27%) |
Thermal Properties | |||
Permanent Linear Change | % | +0.75 | +1.0 |
After heating at Temp. | oC | 1500 | 1200 |
Thermal Conductivity at1000 oC | kcal/hr.m.oC | 2.70 | |
Chemical Properties | |||
Alumina (Al2O3) | % | 45.0 | 45.0 |
Iron Oxide (Fe2O3) | % | 1.0 | 1.2 |
Silicon Carbide (SiC) | % | 25.0 | 23-27 |
Physical Properties | |||
Cold Crushing Strength at 110oC | kg/cm2 | 700 | 700 |
Dry Density | g/cm3 | 2.64 | 2.65 |